MACOR® Machinable Glass Ceramic Thermal Properties

Thermal Properties

SI/Metric

Imperial

Expansion Coefficient
— –200°C to 25°C

74x10–7/°C

41x10–7/°F

— 25°C to 300°C

93 x10–7/°C

52 x10–7/°F

— 25°C to 600°C

114 x10–7/°C

63 x10–7/°F

— 25°C to 800°C

126 x10–7/°C

70 x10–7/°F

Specific Heat

(25°C) .79 kJ/kg • °C

.19 Btu/lb • °F

Thermal Conductivity

(25°C) 1.46 W/m • °K

10.16 Btu • in/hr • ft2 • °F

Continuous Use Temperature

800°C

1472°F

Maximum Use Temperature

1000°C

1832°F

 
Macor Thermal expansion and Macor thermal conductivity vs temperature curves