Aluminum Nitride Substrate Properties
& Physical Characteristics
|
Substrate Physical Characteristics
|
|
Surface Condition
|
Attribute(s)
|
Tolerance
|
|
As-Fired |
Length & Width |
+1%, NLT
+.005" |
|
Thickness
|
+10% |
|
Camber
|
.003"/inch
|
|
|
|
|
Lapped |
Length & Width |
+1%, NLT
+.005"
|
|
Thickness
|
+.002" |
|
Camber
|
<.002"/inch
|
|
Aluminum Nitride Substrate Material Properties
|
|
Property
|
Units
|
Value
|
|
Density |
g/cc
|
3.3 |
|
Thermal Conductivity |
W/m°K
|
170 minimum
|
|
Dielectric Strength |
kV/mm
|
20
|
|
Thermal Expansion |
ppm/°C
|
4.6
|
|
Volume Resistivity |
ohm-cm
|
1014
|
|
Dielectric Constant |
|
9.0
|
|
Flexural Strength |
MPa
|
450
|
|
Reported values are at room temperature
|
You can request a quotation for standard substrate sizes or
custom components at our Aluminum
Nitride RFQ page.
See also: Materials > Aluminum Nitride
|
 |
|
Standard Products | Custom
Products and Services | Case
Studies | Materials
Design Notes
| Working Together |
Vision | Contact Us |
Site Map
1-908-213-7070
© 2013 Accuratus
Site Design M. Adams
|
|
|
|
|