MACOR Machinable Glass Ceramic Bar Sizes

Macor® machinable glass-ceramic is available in a wide range of standard shapes and sizes. It can be purchased as rods, sheets, bars and discs. Stock sizes are normally available from stock for immediate delivery.  Don't see what you need?   Be sure to contact us with your special sizes or send your drawings for quotation.  Custom sizes are our specialty!

Standard MACOR Bar Sizes
SI Units
 
Imperial Units
 
Millimeters
Fractional Inches
Decimal Inches
 
Height
Width
Length
Height
Width
Length
Height
Width
Length
 
6.3
6.3
76
 
1/4
1/4
3
 
.250
.250
03.000
 
152
6
06.000
 
305
12
12.000
 
9.5
9.5
76
 
3/8
3/8
3
 
.375
.375
03.000
 
152
6
06.000
 
305
12
12.000
 
12.7
12.7
76
 
1/2
1/2
3
 
.500
.500
03.000
 
152
6
06.000
 
305
12
12.000
 
19
19
76
 
3/4
3/4
3
 
.750
.750
03.000
 
152
6
06.000
 
305
12
12.000
 
25.4
25.4
76
 
1
1
3
 
1.000
1.000
03.000
 
152
6
06.000
 
305
12
12.000
 
31.75
31.75
76
 
1-1/4
1-1/4
3
 
1.250
1.250
03.000
 
152
6
06.000
 
305
12
12.000
 
38.1
38.1
76
 
1-1/2
1-1/2
3
 
1.500
1.500
03.000
 
152
6
06.000
 
305
12
12.000
 
50.8
50.8
76
 
2
2
3
 
2.000
2.000
03.000
 
152
6
06.000
 
305
12
12.000
 
     


Macor
Bars | Discs | Rods | Sheets

Standard Products | Custom Products and Services | Case Studies | Materials
Design Notes | Working Together | Vision | Contact Us | Site Map

1-908-213-7070

©2002 Accuratus

Site Design M. Adams