Aluminum Nitride Substrate Sizes

    Substrates can be ordered by part number or size.  You can go to our Aluminum Nitride Request for Quotation page and fill out an on-line request or call us at 908-213-7070 for immediate service.

Part Number Designation

Substrate Part Number Designation

* See Aluminum Nitride Substrate Characteristics for physical attributes and tolerances.
Standard Aluminum Nitride Substrate Sizes
Part
Number
Width 

Length
Thickness
Surface
In Stock



2020.025-L
2" 2" .025" lapped
2020.040-L
2" 2" .040" lapped
Available




2020.025-F
2" 2" .025" as-fired
2020.040-F
2" 2" .040" as-fired
2020.060-F
2" 2" .060" as-fired
3030.025-F
3" 3" .025" as-fired
3030.025-L
3" 3" .025" lapped
3030.040-F 3" 3" .040" as-fired
3030.040-L 3" 3" .040" lapped
3030.060-F 3" 3" .060" as-fired
4545.025-F 4.5" 4.5" .025" as-fired
4545.025-L 4.5" 4.5" .025" lapped
4545.040-F 4.5" 4.5" .040" as-fired
4545.040-L 4.5" 4.5" .040" lapped
4545.060-F 4.5" 4.5" .060" as-fired
5070.025-F 5" 7" .025" as-fired
5070.025-L 5" 7" .025" lapped
5070.040-F 5" 7" .040" as-fired
5070.040-L 5" 7" .040" lapped
5070.060-F 5" 7" .060" as-fired



See also: Materials > Aluminum Nitride

 

Standard Products | Custom Products and Services | Case Studies | Materials
Design Notes | Working Together | Vision | Contact Us | Site Map

1-908-213-7070

©2009 Accuratus

Site Design M. Adams